In order to facilitate the long-term tracking and positioning management of buried natural gas pipelines, it is necessary to test the performance of the tracer wire to select a more appropriate tracer wire. Therefore, we have tested the commonly used tracer wire in gas pipelines to provide reference for the selection of tracer wire in natural gas pipelines from the aspects of tracer wire conductivity, anti-corrosion treatment of tracer wire joints, and tracer wire strength.
Test overview
First, the copper-clad steel, copper core wire and copper-clad aluminum are buried above the same PE gas pipeline. The total length of PE pipe is about 717m, and then the conductivity and corrosion resistance of the joint are tested. Performance and strength, followed by data analysis, comprehensive evaluation of the tracer.
Test items
① PCM pipeline current decay rate method is used to test and evaluate the conduction of various trace line pairs;
② Test the anti-corrosion treatment of joints during the construction of various trace lines, and evaluate whether the trace lines can keep the connection from corrosion and fracture after long-term burial;
③ Test and evaluate whether the three tracer wire are buried on a PE gas pipeline at the same time, and whether the spatial position of the pipeline can be accurately located.

Test data analysis
① The systematic analysis of the test data shows that there is no significant difference in the signal conduction of the test current under the same crossing conditions for the three kinds of trace wires: copper-clad steel, copper core wire and copper-clad aluminum. Sectional area. The routing conductive signals of the two aluminum clad wires are almost the same, and the routing conductive signals of the copper core wire are slightly better, but there is no significant difference.
② There are great differences among the three kinds of fuel gas tracer wire in the anti-corrosion treatment of joints. During the test, there were leakage problems at the joints of the three trace wires, especially the copper-clad aluminum, with many leakage joints. If these leakage points are buried for a long time, the tracer wire will be corroded and disconnected, and the tracing effect on the pipeline will be lost. After good anti-corrosion treatment, only one leakage problem was found in the copper core tracer wire joint, followed by the copper-clad steel tracer wire.
The above is the relevant content of the question answer. I hope it can help you. If you still have any questions about this problem, you are welcome to follow our website http://webtest2.daoshangbao.cn And consult our staff, will serve you wholeheartedly.